(264b) Nanoscale Patterning With S-Layer Proteins And Area Selective Atomic Layer Deposition

Authors

Jiurong Liu - Presenter, University of California at Los Angeles
Carey M. Tanner - Presenter, University of California at Los Angeles
Esther Lan - Presenter, University of California at Los Angeles